Cracking in Concrete
Random cracking can:
- make
concrete look ugly
- lead to structural weakness.
Bad cracking leaves the steel reinforcement
exposed to air and moisture, which may cause it
to rust and weaken the concrete.
Reinforcement and joints are used to control
cracking.
(See Joints and Reinforcing.)
Types of cracks
Two types of cracks happen in reinforced concrete:
- Pre-set cracks: Cracks that happen before concrete hardens,
while it is still workable.
- Hardened cracking: Cracks which happen after concrete hardens.
Reasons for cracking:
- Pre-set cracks:
Pre-setting cracks are cracks which form during placing, compaction and finishing caused
by movement of concrete before it is dry.
There are three types of pre-setting cracks:
- Plastic settlement:
When ? They form soon after
concrete is placed, while it is still plastic. They
get bigger as concrete dries and shrinks and
tend to follow the lines of reinforcement.
Prevention:
- Revibrate the concrete.
- Re-trowel the surface.
- Look for cracks as the concrete is
setting. At this stage they can easily
be fixed.
- Plastic shrinkage:
When ? On very hot days or in low humidity and moderate winds. Cracking
is more common in summer but may occur during winter.
(See 12 Hot and Cold Weather Concreting.)
Plastic shrinkage cracks appear in lines,
roughly parallel or in a crazed haphazard
way. They are usually 300–600 mm long but
may be between 25 mm and 2 m in length.
Prevention:
- Dampen the subgrade and forms, and protect
concrete from the wind.
- Keep all materials cool on hot days
- Place, compact and cure as quickly as possible on hot days so concrete won’t dry out.
- Once the concrete has been compacted, screeded and floated apply a uniform spray film
of evaporative retardant (aliphatic alcohol) to prevent rapid loss of surface
moisture, then continue with finishing.
- Try to place at the cooler times of the day.
Repair:Cracks may be closed by reworking
the plastic concrete.
- Formwork movement: caused by movement of the formwork.
If formwork is not strong enough it may bend or bulge. Formwork movement may happen
at any time during placement and compaction.
Prevention: Make sure formwork is strong.
If the concrete collapses, strengthen the formwork and re-vibrate the concrete.
Thermal Shock:
Applying cold water, as curing, over concrete on a hot day can result in cracks from the
sudden contraction.
Prevention: Use warm water.
Pre-setting cracks can be prevented by looking for them as they happen, while the
concrete is still setting.
If they are detected early on they can be easily fixed by re-compacting, re-trowelling or
re-floating the concrete surface.
- Hardened cracking:
Cracks after hardening may be caused by:
- drying shrinkage
- movement or settling of the
ground
- placing higher loads on the concrete than it was designed to carry.
Little can be done with cracks after hardening. Careful and correct placement helps
prevent serious cracking after hardening.
Only uncontrolled cracks are a possible problem. Cracks at control joints or controlled by
steel reinforcing is expected and acceptable.