Welding - intro
Sources
Sources include lecture notes, notes taken in practical classes, notes from textbooks long misplaced, CIG manuals, Liquid Air (Aust) manuals, and the internet:
welder's corner
http://www.dansworkshop.com
http://autospeed.com
http://www.gowelding.org
and there's more ... .
You should visit these sites instead of this one because they have more to offer. This site is for underprivileged students using legacy computers and primitive internet connections. They therefore cannot access the large files on normal websites, which use over 3MB per page (with illustrations) compared to 30KB on this site.
Glossary
Inclusions: slag (dead flux) trapped inside your weld. Ruins the join.
Penetration: To penetrate properly the molten metal must melt the far side of the job, filling the groove completely, without slag inclusions.
Contents
Contents:
- SMAW - Shielded Metal Arc Welding: thick wire electrode covered in flux which burns to shield molten metal.
- DC welding machine
- AC welding machine
- GMAW - Gas Metal Arc Welding - MIG welding: fed by coiled wire and shielded by bottled gas
- FCAW - Flux Cored Arc Welding: as for MIG but flux inside wire burns to shield wire
- GTAW - Gas Tungsten Arc Welding - TIG welding: with a tungsten non-consumable electrode, wire fed by operator's other hand and bottled gas to shield wire.
- Accessories
- Electrodes
- Preparation
- Technique
- Gas welding
- Gas Brazing
Welding metal can repair damaged or fabricate new equipment.
Farmer's choice:
- stick welding machines, about 225 amperes capacity and either alternating current AC or direct current DC; cheap, very convenient.
- MIG (metal inert gas with a wire-feed unit & gas shield) for ease of use.
SMAW - Shielded Metal Arc Welding
Shielded Metal Arc Welding, usually called 'stick welding', being the cheapest to set up, is the most common. Stick welding uses 2 types of power sources:
These will be discussed next under separate headings.
DC welder
The DC rotary machine is popular but costs more initially to pay for the electric motor or small petrol or diesel engine to drive the generator. However, some can be driven by existing farm machinery but you would need to try before you buy, since the tractor might not have enough power to counteract the back-emf. (I was amazed how a little welder could almost stall a big tractor.)
DC welders tend to give a more stable arc, and are often in mobile units suited to on-site fabrication or field jobs. However, AC welders are now compact (if your extension cord will reach).
In DC welding, the current has polarity, that is, flows in only one direction. One cable clamps onto the metal you are welding, while the other holds the electrode. Is your electrode positive (+) or negative (-) ? You can flip a switch to change, (on some welders you change the cables over) but you must decide since the flux will accept only one direction. That is, the flux demands that the electrode be positive, or the flux demands that it be negative. You cannot argue with the flux. The package containing the electrodes states which way to do it.
AC welder
An AC welder is a large transformer with a number of tappings to change the level of current for different diameters and types of welding rod. Most farm welding jobs can be done with currents between 100 and 225 amperes of current.
Problems are:
- the need for a live AC socket near the job
- not all AC electrodes work well on a limited input AC welder, partly because of its low open-circuit voltage
- does the welder provide an auxiliary output (socket) for lights, drill, grinder, etc ?
- if the farm-house is a long way from the last mains transformer, and the shed a long way from the farm-house, and the welder on a long extension lead, the total resistance in the line may reduce the voltage too much for the welder to work efficiently.
The electrode packet gives information on which currents to use for which diameter, which current to use (AC or DC), and what type of flux it is (this determines its suitability for the job you are doing).
I always stock a range of electrodes, and protect them from damp by storing in the airing cupboard above the hotwater cylinder.
GMAW - MIG welding
MIG Welding is a slang term that stands for Metal Inert Gas Welding, but the proper name is Gas Metal Arc Welding or “GMAW”, and it is also commonly referred to as “Wire Wheel Welding” by Unions. Low voltage units are now available, and ideal for farm work. For light new work MIG is the best. Finite controls allow the welder to join very light sections. MIG Welding is commonly used in shops and factories. It is a high production welding process that is mostly used indoors.
Metal Inert Gas welding, MIG, is easy to learn for a beginner but requires an inert gas (Argon or a mixture) to act as a flux; which always seems to run out in the middle of a job.
MIG Welders have five main components:
- constant voltage power supply
- wire feed to feed the filler wire through the welding lead to the MIG gun
- ground lead or clamp
- welding lead or MIG gun
- Shielding gas to protect the weld area from the air.
MIG welding is not that simple when it comes to setting up the equipment but the skill required is a lot less then Stick welding.
Method:
- attach the ground clamp to the work
- turn on the power source
- turn on the shielding gas
- set the voltage
- set wire feed speed that is counted in IPM (inches per minute)
- set shielding gas flow rate that is counted in CFH (cubic feet per hour)
- hit the trigger and the MIG gun starts feeding shielding gas and wire to the weld joint
- once the wire hits the weld joint it begins to arc and the wire melts and starts filling the joint.
The problems are:
- dirty work, with old paint, rust or scale, make welding difficult
- the gas shrouds the weld but does not pick the contaminants and wash them away like electrode flux does (within reason)
- outside jobs can be difficult when the wind interferes with the argon stream
- welding light metal to heavy metal is hampered by the heavy metal not heating sufficiently to melt and bond (called 'cold overlap'). The problem can be that the wire is too heavy, say 1.2mm, when 0.9 would create a hotter weld pool. Bigger is not always better.
FCAW - Flux Cored Arc Welding
Flux Cored Arc Welding “FCAW” is a MIG welder with a different welding wire (electrode).
FCAW wire is a hollow or tubular wire that has a flux inside of it that provides a shielding from the air when it is welding. What this does is help a MIG welder to weld in windy conditions and it increases how much weld can be welded per hour. The powder flux inside also has metal mixed in that increases the weld deposit rate.
FCAW is the fastest of all of the manual welding processes. FCAW wire has two types:
- Self Shielding: has enough flux inside that no other shielding source is needed.
- Dual Shielding: helps shield the weld but also needs a source of gas just like a MIG welder.
Flux cored arc welding has a slag like Stick welding; a slag which must be removed.
GTAW - Gas Tungsten Arc Welding - TIG welding
TIG (Tungsten Inert Gas) Welding or HeliArc Welding are the slang terms for GTAW - Gas Tungsten Arc Welding. TIG welding is the most difficult of the processes to learn, but is the most versatile when it comes to different metals. This process is slow but can produce the highest quality weld. TIG welding is mostly used for:
- critical weld joints
- welding metals other than common steel
- where precise, small welds are needed.
TIG welders have six main components:
- constant amperage power source (many times a Stick welding power supply)
- ground lead or clamp
- welding lead or TIG Torch
- non-consumable Tungsten electrode to produce the arc (the Tungsten electrode does not add to the weld joint)
- shielding gas to protect the weld area from the air (typically pure Argon gas)
- filler wire to add to the weld joint with the other hand.
The simplest TIG welder is nothing more than a Stick welding machine with a TIG torch and a hose to a bottle of Argon gas. This technique is commonly used in industry.
The process is simple:
- attach the ground clamp to the job (metal to be welded)
- insert a Tungsten electrode into the TIG torch
- turn the Argon gas regulator on and the TIG torch gas valve
- scratch the Tungsten on the job to strike an arc
- the Tungsten electrode produces an arc and starts to melt the metal
- add filler wire to the joint with the other hand.
Accessories
Choose accessories carefully:
- Insulated holders are worth the extra cost.
- Electrode and arch cables should never be longer than the manufacturer recommends because they only get hot and waste energy.
- Never operate with the cable coiled, and, even worse, coiled around a drum. It can become so hot that it fuses together.
- Ground clamps must be treated respectfully and be rated as high as the maximum welding current of the welder.
- A good head shield is necessary to protect the operator from arc spatter (try overhead welding - I have yet to find one that good). The inner lens must absorb all infrared and ultraviolet rays, and the outer lens must be chemically treated clear glass to protect the colored glass against spatter. Spares should be kept in store, so they can be changed when damaged, to maintain clear vision. Never use a cracked lens.
- Greenskin leather protects against arc sparks setting alight to your clothes - it happens and you scar before you realize. Leather steel-capped boots with leather gaiters to prevent sparks from falling down inside the boots.
- chipping hammer, wire brush, files and welding table. I use blades from machine hacksaws, sharpened into points, to cut away any slag inclusions.
Electrodes
Electrodes are made in different diameters, of different metals, with different chemical coatings (flux). The diameter of the core wire determines the size of the electrode.
The chemical flux coating on the electrode has several functions and largley determines how the electrode will act during welding.
The burnt flux forms a smoke blanket of gas which acts as a shield around the arc and pool of molten metal to protect them from the surrounding air.
Electrodes are identified by a system of classification numbers adopted by the Australian Standards Association. Manufacturers then print the classification or name the flux coating to identify these various classes.
Generally the more heat you can get into the weld pool (molten metal) the easier it is to weld (for the non-professional).
The secret is to concentrate your mind into the swirling pool of molten metal.
Low-hydrogen electrodes produce a better weld for the unskilled, but check the packet information to see if they will run on your welder. In addition these low-hydrogen electrodes are used on hard-to-weld steels, such as higher carbon content steels, alloy steels, spring steels, armor plate, car bumpers.
Some rods (electrodes) are twin coated to give beginners a better weld: the inner coat is the standard low-hydrogen whle the outer is an iron powder.
General purpose electrodes are designed for the novice, but others have a fast freeze flux which are less forgiving, increasing flux cavities and inclusions which must be removed. The fluxes which are slower to freeze are easier to use. However, fast-freeze has its purpose: in such welds as vertical down-hand, the molten metal and flux tend to stay behind the weld as you travel down.
To weld a forging or casting requires special care.If it will need to be machined afterwards, then special rods will be needed. Preheating will make welding easier. The best is a blacksmith's forge, immersed in the coals of the fire. Allow the job to cool slowly, even if you weld away from the preheat, then put it back so all the metal contracts evenly.
Stainless steel will not absorb any of the carbon in the metal being welded. They are good for welding tynes back on forks. Try preheat, SS rods and postheat.
Preparation
Preparation is (almost) everything.
Haste will cause:
- Inclusions (dead flux trapped inside your join) that are time-consuming to remove, and remove them you must.
- Distortion/warping of the metal around the join, or a wedged-shaped weld. Requires a new attempt, thus wasting metal and time and electrodes and power.
- Uneven welds with blobs of metal hanging off; requiring grinding.
Welds last forever, for everyone to see and to ruin your reputation and embarrass you.
Preparation usually takes longer than the actual welding:
- Thick metal should be bevelled to let the tip of the rod down near the far side of the metal. This, with the edges spaced apart, allows the arc to melt the metal to the far side of the join, so the weld is slghtly thicker than the metal being welded, and without inclusions.
- Broken pieces should have enough edge left to anable the 2 edges to be re-aligned and the original dimensions retained.
- The edges and the face along the edge should be spotless - no dirt, no grease, no rust. Wipe, wire brush and grind it off. When spotless, there will still be some left but the flux is designed to remove tiny amounts.
- If there are gaps or extra holes along the edge, with possibility of the arc burning through the gap, thus forming a bigger hole, then place a backing plate behind. If the backing plate can be left in place as part of the job, then it becomes part of the weld. Otherwise use copper as a backing plate because it does not easily adhere.
- Allow for the intense heat buildup in the metal, causing distortion (bending and warping):
- Avoid over-welding, and use as little weld metal as possible for the necessary strength. There should not be a groove along the edge of the weld, and the weld should be either flat or with a slight smooth swelling.
- I insert spacers in the crack between the two sides, then tack (a short weld deep in the groove) The spacers prevent the weld from closing the crack. Knock the spacers out, then do short welds every few inches. Remove the flux completely. Then do staggered short runs, so that each cools while the next is being done. This reduces bending and warping. If the 2 pieces are closing up, hammer them apart again. Using a ball peen hammer inside the weld itself will expand the weld, allowig the pieces to open.
- Prepare the metal properly, clean, bevelled edges, with spacers, slightly over-open to allow for contraction of weld metal.
- Use intermittent welding where possible, short beads with space between when the full strength of a long weld is not needed.
- Run short passes and allow them to cool before adding the next.
- Use the backstep method by which each pass is started ahead and run back into the previous weld.
- Locate parts out of position and allow the weld bead to pull them back into position whenit contracts.
- With long filler welds, balance the contraction of a bead on the other side.
- Carefully hammer or peen a weld deposit ehough to make up for contraction on cooling.
- Hold the job in a jig, or with clamps or a vice for support during welding and cooling.
Technique
Technique:
- When the shield goes down over your face you cannot see anything, so before that:
- Hold the rod close to the work, ready to weld.
- Drop the shield over your face with your free hand.
- Strike an arc near the beginning of your weld, to give you enough light to see, then hold it about 10mm long for a second or two till you locate the precise point to begin welding.
- Shorten the arc to about 3mm. The correct length of arc gives a sharp crackling sound like bacon frying (my apologies to Jew and Muslim welders).
- Hold the electrode at the start long enough to penetrate properly (molten metal must melt the far side of the job). Deposit enough metal to establish the size of the bead before moving on.
- If your rod fuses to the job and cannot be pulled off, release the electrode from its holder immediately. Do not remove or lift your headshield until the rod has been freed from its holder. Wait for the rod to cool before using piers to break it free. Put the rod back into its holder. If flux has broken off leaving the end of the rod bare, drag the rod across earthed scrap metal till the rod melts down to the flux; then continue the job.
- Use your weld bead to determine your strong and weak points:
- A normal bead, the result of correct amperage, arc length and speed, is smooth, slightly swollen, with fine ripples - it looks good, has good penetration, good fusion at the edges, no porous gas holes in the surface and no slag induced in the weld.
- A cold bead, caused by too low amperage, piles up on top of the job, with poor penetration and fusion, and the arc is hard to maintain.
- A hot bead, with its long crater, too deep a penetration, with excessive spatter.
- Travel too fast, gives a small bead, irregular with elongated ripples
- Travel too slow, causes a wide bead and overlay as too much metal is deposited.
- Too long an arc gives a flat bead, poor penetration, irregular width and excessive spatter.
- To give a wide bead, weave side-to-side slightly.
- Where a weld is inside a corner, counting helps, with -1- counted on the edge and -2-3- in the middle, and again -1- on the edge, so the rod spends more time in the middle of the angle than at the edge of the weld.
- Watch the experts and ask advice.
Gas welding
Combustible gases inlude oxygen-acetylene, oxy-LPG, air-fuel (usually LPG).
The oxy-acetylene cutting and welding set consists of 2 cylinders, one of oxygen O2 and one of acetylene C2H2.
The gas acetylene is made by adding water H2O to calcium carbide Ca C<