MIG
Go Welding.Org. © 2008 - 2012 All rights reserved.
Advice 1
We all talk about current flowing through circuits from the positivve terminal to the negative terminal – but there is no such thing as a current.
Electricity is the flow of electrons, tiny negative charges which flow from negative to positive.
For this reason I use the term 'electron-flow' where others use 'current'.
Advice 2
This chapter is an edited version of that found on Welding.org. If you can access that website, please do. It has many more articles, and those are illustrated with colored photographs. This site is for underprivileged students with poor internet connections which require brief download times. Thus they are unable to use welding.org because its articles are too large (3.4MB to this 40KB). You are slowing their downloads, risking a dropped connection. If you re-address, then thank you.
What is MIG Welding ?
MIG welding is an abbreviation for Metal Inert Gas Welding. It is considered semi-automated in that the welder still requires skill, but that the MIG welding machine continuouslyfills the joint being welded.
MIG welding machines consist of a handle with a trigger controlling a wire feed, feeding the wire from a spool to the weld joint. The wire runs through the liner, which also has a gas feeding through the same cable to the point of arc, which protects the weld from the air.
MIG welding is most commonly used in fabrication shops where production is high, and protected from wind blowing away the shielding gas.
How MIG Welding Works
MIG weld welding requires three things:
- electricity to produce heat
- an electrode to fill the joint
- a shielding gas to protect the weld from the air.
MIG welding is done using a very small diameter electrode that is fed continuously, while the operator controls the amount of weld being done. In some cases when a robot takes over this process, it becomes automatic welding.
MIG Voltage Type and Welding Polarity
MIG welding, unlike most other welding processes, has one standard voltage type and one polarity type. The voltage used is DC direct current, much like the current in a car battery, with electrons flowing in only one direction. These electrons flow from the negative (-) terminal on the MIG machine to the positive (+) terminal.
The polarity used is also standard; the DC electrode is positive (+). The handle is the positive side of the circuit. The electrons flow from the metal of the job being welded, into the positive (+) welding handle.
The power source used for MIG welding is called a “constant voltage power supply”. In MIG welding the voltage is what is controlled and adjusted. When comparing MIG welding to Arc or TIG welding, MIG welding machines use voltage settings to set the machine. TIG and Arc welding machines use amperage to set the machine or a “constant amperage power supply”.
MIG Electrode Types
When choosing the proper MIG wire or electrode you need to match the type of wire to:
- the type of metal being welded
- the type of transfer
- position to be welded
- resistance to abrasion.
For the factory, the welding engineers specify the weld size and electrode type to be used.
The most common wire used for welding carbon steel is ER 70S-6. In some cases you can weld two different metals together. An example of this is welding 304 stainless steel to A36 carbon steel using an electrode made of 309 stainless steel “ER 309L”.
Typical MIG welding electrodes are a solid wire ranging from a thickness of 0.023" to 0.045". Some are much thicker for heavy industrial applications. The most common sizes are:
- 0.023"
- 0.030"
- 0.035"
- 0.045"
MIG Welding Wire
The manufactures of these electrodes use a standard code to identify the type of electrode. For example the code on the label ER 70S-6 represents the following:
- ER - An electrode or filler rod that is used in either a wire feed or TIG welding
- 70 - A minimum of 70,000psi (483MPa) of weld tensile strength (1MPa = 145psi)
- S - Solid wire
- 6 - The amount of deoxidizing agent and cleansing agent on the electrode.
Common MIG Welding Gases
Gas for MIG welding is what makes MIG welding possible. The name informs us of this; “Metal Inert Gas welding”. The gases shield the weld from oxygen in the air. When Carbon Dioxide or Oxygen is added to the mixture, MIG welding is not technically MIG welding anymore. This is due to the fact that both Carbon Dioxide and Oxygen are not inert gases. The process then becomes GMAW or Gas Metal Arc Welding.
The type of gas uses also determines:
- how deep the weld penetrates the metal welded
- the characteristics of the welding arc
- the mechanical properties of the weld.
When choosing the type of gas to be used, it is best to seek input from a welding supply store. The store will recommend the proper gas to match the welding wire to be used. Or, you can use the welding wire manufacturer's recommendation. Typically, the manufacturer will provide a few choices ranging from the best choice, to the gas that will provide the minimum cost but with the minimum acceptable results.
The four most common gases used are:
- Argon Ar
- Carbon Dioxide CO2
- Oxygen O2
- Helium He (the least common)
Mostly these gases are used as mixtures, typically carbon dioxide with Argon or Oxygen. Oxygen causes most weld defects, but in small percentages, mixed with other gases, it improves the arc characteristics. Argon and Carbon Dioxide can be used by themselves. In some cases there is tri-mix shielding gas containing Ar + CO2 + He, or, Ar + CO2 + O2.
The more common mixtures and gases are:
- label C2 = 2% Carbon Dioxide and 98% Argon
- label C25 = 25% Carbon Dioxide and 95% Argon
- 100% Carbon Dioxide (cheapest)/li>
- 100% Argon
Some basic guidelines for choosing the appropriate gas are as follows:
- Welding of carbon steel can be done with Carbon Dioxide alone and it produces the deepest penetration, the most smoke and the roughest weld. A mixture of gases ranging from 2% to 25% Carbon Dioxide and the rest Argon can be used. A higher percent of Argon improves the arc characteristics and gives a smoother, better looking weld.
- Welding of stainless steel is typically done with C2 or 2% Carbon Dioxide and 98% Argon. In some cases there is tri-mix shielding gas containing 90% Helium, 7.5% Argon, and 2.5%Carbon dioxide.
- Welding of Aluminium is typically done with Argon alone, with one exception. If the Aluminium being welded is thicker then ½ of an inch there may be Helium added to the mix.
Argon gas by itself works well on most exotic metals like:
- Copper & copper alloys
- Magnesium
- Nickel & nickel alloys
- Titanium
MIG welding transfer types
MIG welding has four ways of transferring the wire to the joint.
These 4 MIG welding transfer types are:
- Short circuit
Short circuit transfer is a transfer used with a lower voltage. Short circuit transfer occurs when the wire arcs and contacts the metal creating short circuits. During this short circuit, the wire contacting the metal heats up and drips into the joint by creating a puddle. Then another arc begins and the process keeps repeating many times a second. The easiest way to tell if the transfer is short circuit is by the sound. The sound greatly resembles an egg hitting an extremely hot frying pan. It is a very crisp and fast crackling sound. Typically short circuit transfer is used on thin metals or sheet metals.
- Globular
Globular transfer is similar to short circuit transfer. Globular transfer like short circuit occurs when the wire arcs and contacts the metal creating a short circuit while melting the wire but the main difference is the wire melts for a longer period of time creating a glob that hangs off of the wire. Then the glob falls to the metal filling the joint and then the process begins again. Globular transfer has a popping sound to it. It has a few pops per second and many times you can actually see the glob being formed and dropped.
- Spray
Spray Transfer is a transfer where a higher voltage is applied. The transfer is exactly like it sounds. The wire sprays or has very fine mist transferring to the metal. The way to tell if you are using a true spray transferring arc is if it has a fine hissing sound and no crackles or pops. There will be a clean arc to the metal without spatter.
- Pulsed spray
Pulsed spray transfer is a transfer that is done with special equipment. The equipment pulses the voltage many times a second, allowing the arc to go between spray transfer, to globular transfer, back to spray transfer and so on.
How to Set Different Transfer Types
If you have never MIG welded it would help to know that there are no settings on a MIG welding machine offering a choice of transfer type. The ways a different type of transfer are set have two ingredients
voltage settings
type of gas.
Most short circuit transfer welding is done with lower voltage and usually using carbon dioxide or a carbon dioxide gas mixture.
Globular and spray transfer use a higher voltage setting and commonly use Aragon gas. The Argon gas may contain a percentage of carbon dioxide, helium, and/or oxygen.
Almost any metal may be MIG Welded.
MIG welding is a welding process that can weld almost any metal. It may not always be the best choice for weld quality but MIG welding is a fast, cost efficient, and produces results that are more than acceptable for most manufacturing and fabrication needs. The three most common metals welded with a MIG welder are:
- carbon steel
- stainless steel
- aluminium, with a special feeder because Aluminium wire is very soft.
MIG Welding Carbon Steel
Carbon steel welds are almost flawlessly done with a MIG welder. There are very few problems, beside the downside of the design of a MIG welding machine. The wire stiffness is just right to pass through the liner from the machine with minimal friction to cause problems and has enough stiffness to feed without coiling up. Depending on how much voltage the MIG welding machine is running at, the weld can be set to one of three transfer types:
- short circuit
- globular
- spray.
MIG Welding Stainless Steel
Stainless steel MIG welding does not require any special equipment. The biggest problem comes from the cord or liner of the welder. The trick when welding stainless steel is to keep the cord as straight as possible. Otherwise, the wire feed will have too much friction due to stainless steel being stiffer than carbon steel.
The wire is so stiff in the liner that it causes such friction that the wire stops the feeding wheel from feeding the joint (literally spinning its wheels). The wire then stops or slows down to the point that the arc melts the wire up to the MIG tip and it welds itself to it. The result is a fused MIG tip.
The other major problem is again the liner. If you bend the cord to much the friction stops the wire and the wheels that are feeding the MIG gun push the wire so hard that the wire, having no place to go, spools before it gets pushed into the liner.
MIG welding stainless steel is mostly done in a spray transfer or globular borderline spray. The reason behind this is that stainless steel does not do to well with short circuit transfers. The short circuit transfer and globular have the wire actually hitting the metal, splashing and splattering, and that also causes friction on the liner.
Welding stainless steel requires a high percentage of Argon used in the gas mixture. If it is a critical joint that will be x-rayed, any disturbance in the transfer will cause flaws. Spray is a smooth crackle-free transfer that has no metal being violently transferred. Spray transfer also keeps spatter to the bare minimum. Stainless steel spatter is extremely difficult to clean.
MIG Welding Aluminium
Aluminium MIG welding usually requires a double feed, referred to as a push and pull method. A spool of wire is pushed through the MIG handle and the handle itself has a pulley that pulls the wire. Welding aluminium is not very common for MIG welding. It is typically done when high production is needed.
Another type of feed that can be used is a spool feed MIG gun. It has a small spool of wire on the MIG gun itself. This type of feed is the most trouble-free of the feeds when it comes to MIG welding aluminium.
When MIG welding aluminium the technique used is always forehand and you need to push the puddle.
MIG welding aluminium is typically done with pure Argon gas using a spray transfer. On thicker joints the transfer has a fast crackle and the weld is very quick. Welding thicker aluminium out of position works well but the weld appearance is never perfect! The aluminium weld in the picture is a single pass and took about 10 seconds to do on a 9mm (3/8") bevel. It’s all about moving quickly and keeping the puddle from rolling over.
MIG Welding Pros
MIG welding has some very good advantages:
- Welds are clean with very little smoke.
- Production is cheap and fast.
- Long welds with fewer restarts.
- The skill level needed compared to other welding processes make it easy.
- Welding wire runs continuously with less down time to replace electrodes.
- Excellent for spot and tack welds.
MIG Welding Cons
MIG welding does have a few problems:
- Distance from the MIG machine to the operator is limited.
- Wind prevents use outdoors.
- Always need a bottle of gas.
- The cable that transfers the spool of wire through it needs to be well maintained.
- If contact tips are spattered, they seize up.
- Needs a clean joint.
- There are many parts to a MIG welder that need to work properly and finding a cause is time-consuming.
Joint Setup and Preparation
With MIG welding it is very critical that the weld area is clean. MIG welding will not be successful with a dirty joint. Unlike some stick welding / SMAW rods that can burn through rust, MIG welding has a lot of difficulties welding dirtier metals. It also does not have slag to protect the weld when the gas is gone. When MIG welding make sure you have a clean joint by removing any foreign substance. With MIG welding a slight bit of dirt or rust is OK but anything more is asking for trouble. MIG welding painted or coated metals does not work well at all.
MIG Welding Machine Set-Up
Set-up of a MIG welder depending on what the type of wire transfer type is chosen. There are three main ingredients:
first the voltage settings, then the wire speed, and finally the type of gas. Almost any type of gas will allow you to spray transfer, but the gas type is what changes the quality of the weld!
First set the gas to flow between 25 to 35 CFH. This is only a guideline! If you are welding indoors you may need less and if you are welding in a place that may have a draft coming through you may need more.
When setting a MIG welding machine there are two major settings:
Before setting up your MIG machine there should be some instructions on the machine itself for the proper voltage on the inside of the panel where the wire goes. This gives the voltage for different thickness of metals. Most of MIG welding is done with the same wire diameter but what changes is the amount of heat the welder requires to heat that metal to get proper penetration of the weld.
The MIG welding machine is best set within the voltage range of what the charts suggest for that metal thickness. The transfer type mostly changes with the wire speed and gas type. When setting your wire speed to the transfer type, listen to the sound of the weld:
- Short circuit has a fast crackle sound
- globular have a few crackles or pops a second
- true spray transfer has just the hum of the welder or hissing sound.
Once you learn the sound, you will know the settings.
MIG welding relies on two major factors:
- joint preparation
- machine set up.
Your weld quality depends on how well you set up your MIG machine!
MIG Welding Techniques
Welders say MIG welding is very easy but that is because they began as arc welders and moved across to MIG with their advanced arc skills. If you are a novice to welding, then you still have to develop basic welding skills and that does not come easily. The secret is to concentrate your mind inside the swirling pool of molten metal.
There are two ways to MIG weld:
- Forehand: push the MIG gun toward the direction of the weld. Forehand welding produces shallow penetration with a flat wide smooth surface.
- Backhand: drag the MIG gun like a Stick welder. This produces a deep penetration weld that is narrow and is high in the center.
To begin welding, the wire should stick out about 20mm. Less is OK but a much longer wire stick out won’t allow the shielding gas to do its job properly.
Some general guidelines for MIG welding techniques are as follows and are only guidelines:
- Flat welding is the easiest. Typically the MIG gun will be pushed, the angle of the MIG gun can be pointing straight down to leaning toward the direction of the weld up to 35 degrees.
- Horizontal welding is a little harder. The MIG gun should be pointing upward between 35 to 45 degrees and tilting about 15 to 35 degrees toward the direction of the weld.
- Vertical down is also pretty easy. You start on the top and work your way down. The MIG gun needs to be tilted up between 35 to 45 degrees. There is a trick to welding vertical down. You need to stay ahead of the puddle and keep the electrode moving from side to side. Otherwise the weld will not penetrate properly.
- Vertical up is a bit harder. The MIG gun handle should be between 35 to 45 degrees. When welding vertical up you need to build a shelf of weld to work upward on. The vertical up weld in MIG is typically very convex. To help with welding vertical up it always a good idea to grind a small grove where you will be welding.
- Overhead MIG welding requires the MIG gun tilted 5 to 35 degrees toward the direction of the weld.
The general guidelines for MIG welding are:
- whip when welding thin metal or making the first pass in a joint
- circles for a both thicker materials and wider welds
- weave for vertical up and down.
My personal preference is to have the voltage at the maximum recommendation and just hold the MIG gun steady letting the MIG gun do the work.
Trouble Shooting MIG Welders
Trouble Shooting MIG Welders:
- Porosity in the weld:
- Check the gas to make sure there is enough left.
- Check the gas flow rate. First raise the flow rate and if that does not work try lowering it. Sometimes too much gas flow causes turbulence by pulling in air to the mix.
- Check the cup of the MIG gun for excessive splatter.
- Check your stick out. It’s common for people who stick weld to allow too much stick out when MIG welding.
- Check the MIG gun for leaks. Typically the MIG gun nozzle may be loose or worn out. Or the gas diffuser may be loose or have spatter blocking the gas flow.
- Change your travel angle. Too much lean toward the direction of the weld can cause air getting pulled into the weld area.
- Check the joint for dirt, water, or any contaminants that should not be there.
- Finally check all of the connections in the gas line for leaks.
- Wire Feed Jams or Uneven Wire Speed:
- Check the MIG tip.
- Check the rollers for proper tension settings.
- Check the rollers for a birds nest.
- Check the wire spool to make sure there is wire left and nothing is catching on it. It’s common for the wire to jam on itself.
- Make sure you are not bending or twisting the liner too much while welding. If not you may need to replace the liner.
- Check the rollers to make sure they are the right size for the wire being used.
- Check the wire connector between the cabal and the wire feeder for a solid connection.
MIG Welding Summary
Carbon steel welds best with MIG because the stiffness of the wire is perfect for the liner. MIG welding is the best choice for spot welding and tack welds. When welding soft metals like aluminium there is special equipment that is needed to be added to the MIG welder. Harder metals like stainless steel work fine on any MIG welding machine as long as you pay attention to keeping the cord straight. Almost any metal can be MIG welded as long as the type of wire and gas are properly chosen.
Most welding techniques that are used for other welding processes still apply here. The whip of a weld, circles, and weaves for wider welds. What changes here is typically the forehand method is used but sometimes the backhand method may be needed. To be an excellent MIG welder, master your machine set-up.